5a03-aluminium-coil is Al-Mg aluminum alloy, the performance of 5A03 aluminum plate is similar to 5A02, but because the magnesium content is slightly higher than 5A02, and a small amount of silicon is added, so the weldability is better than 5A02, the welding performance of 5A03 aluminum plate with gas welding, argon arc welding, spot welding and roll welding is very good, and there is no big difference between the other properties. 5a03 belongs to Al-Mg alloy.
5a03-aluminium-coil is widely used, especially in the construction industry, and is the most promising alloy. Good corrosion resistance, good weldability, good cold workability, and moderate strength. The main alloying element of 5052 is magnesium, which has good forming performance, bell resistance, weldability and moderate strength
Specifications of 5a03-aluminium-coil
| Aluminium alloy | 5a03-aluminium-coil |
| Material temper | F, O, H12, H16, H19, H28, H32, H34, H36, H38, H111, H112, H114, H116, H321 |
| Thickness (mm) | 0.2-500 |
| Width (mm) | 20-2650 |
| Length (mm) | Customized |
| Delivery Terms | FOB, CFR, CIF |
Chemical Composition of 5a03-aluminium-coil
| Elements | Mg | Si | Fe | Cu | Mn | Zn | Ti | Others | Al |
| Content | 3.2-3.8 | 0.50-0.8 | 0.5 | 0.1 | 0.3-0.6 | 0.2 | 0.15 | 0.05 | Remain |
The strength of 5a03-aluminium-coil is equivalent to that of 5A05, the plasticity is high in the annealed state, and the plasticity is moderate during hardening. 5A05 aluminum alloy plate sheet uses hydrogen atom welding, spot welding, gas welding, argon arc welding, good welding performance, high corrosion resistance, anodizing treatment is required when manufacturing rivets.


5a03-aluminium-coil Heat treatment specification:
1) Homogenization annealing: heating at 460~475℃; heat preservation for 12~14h; air cooling.
2) Rapid annealing: heating 350~410℃; holding time 30~120min; air or water cooling.
3) High temperature annealing: heating 350~420℃; when the thickness of the finished product is ≥6mm or <6mm, the holding time is 10~30min or 2~10min; air cooling.
4) Low annealing: heating 250~300℃; holding time 1~2h, air cooling.
Hot Tags: 5a03 aluminium coil 0.4mm thickness, China 5a03 aluminium coil 0.4mm thickness manufacturers, Rust resistant aluminum 5754, 5 series Aluminum Coil, 5052 Aluminum Coil, 5083 aluminum roll, 5083 Aluminum Coil, 5052 alloy aluminum roll