Aluminum Grades and Classifications: 1xxx to 8xxx Series and Temper Codes

How the Aluminium Grade System Works

Aluminium is classified first by composition and then by processing route. Commercially pure metal and its alloys are separated into wrought and cast families, and the wrought family is further divided by the alloying element that dominates the composition. The four-digit designation registered internationally, and mirrored in GB/T 3190, is the practical language that buyers, extruders and rolling mills use to place an order.

In the four-digit system the first digit identifies the alloy group. The remaining digits distinguish individual alloys within that group. A letter inserted after the first digit marks a national variation of the original alloy, and a temper suffix added after a hyphen records the heat treatment or strain-hardening state the product is supplied in.

The Series by Alloying Element

Series Main alloying element Key character Common grades
1xxx None, aluminium 99.00% minimum Highest conductivity and corrosion resistance, lowest strength 1050, 1060, 1100, 1235
2xxx Copper High strength, lower corrosion resistance, needs protection 2011, 2024, 2A12
3xxx Manganese Moderate strength, good workability and corrosion resistance 3003, 3004, 3103
4xxx Silicon Low melting point, used in brazing sheet and filler wire 4043, 4045
5xxx Magnesium Good strength with excellent corrosion resistance in marine use 5052, 5083, 5754
6xxx Magnesium and silicon Extrudable, medium strength, hardening phase Mg2Si 6060, 6061, 6063, 6082
7xxx Zinc Highest strength, used in aerospace and high-load parts 7075, 7050
8xxx Other elements, often iron or lithium Special duties such as foil stock and low-density alloys 8011, 8079

Grade 8xxx is not a single family in the way that 6xxx is; it collects alloys whose principal addition falls outside the elements used to define the other groups. A ninth group is kept in reserve for alloys introduced later, and is not in commercial use today.

Wrought and Cast Alloys, and Legacy Designations

Wrought alloys are intended for pressure working such as rolling, extruding, forging and drawing, and they hold good plasticity in the as-cast condition. Cast alloys are shaped directly by pouring into a mould, and they are grouped by the dominant addition: aluminium-silicon, aluminium-copper, aluminium-magnesium and aluminium-zinc systems. The aluminium-silicon family dominates casting because it combines good fluidity with low shrinkage.

Older Chinese designations remain in circulation on drawings and in legacy stock lists. Industrial pure aluminium was once identified as L1 through L6, covering a purity band from roughly 99.7% down to about 98.8%. Wrought alloys used the letters LF for rust-proof grades, LY for hard grades, LC for super-hard grades and LD for forged grades. These codes are still encountered in maintenance and reverse-engineering work, so a translation table is worth keeping alongside the current four-digit system.

Temper Designation and Why It Changes Everything

Two products carrying the same grade can behave very differently because of temper. The suffix after the hyphen records the treatment:

F as fabricated, no special control of mechanical properties

O annealed to the softest, most ductile condition

H strain hardened, with a second digit describing the hardening level, as in H14, H24 or H18

W solution heat treated and unstable, used only for short-lived interim states

T thermally treated to a stable condition, with a second digit recording the sequence, as in T4, T5, T6 or T651

A 6061-T6 extrusion and a 6061-O extrusion share a chemistry but not a strength. The temper therefore belongs in the specification next to the grade, not as an afterthought. EN practice adds the EN AW prefix, so the same material may appear as EN AW-6061 T6 in a European enquiry and as 6061-T6 in a Chinese or American one.

Selecting a Grade in Practice

Start from the service environment: marine and coastal work points to the 5xxx series, where magnesium gives corrosion resistance with useful strength.

Where formability and conductivity matter more than strength, such as busbar, foil stock and heat transfer parts, the 1xxx series is the natural choice, with 3xxx grades when slightly more strength is needed.

For extruded profiles, frames and formwork panels, the 6xxx series offers the best balance of extrudability, strength and surface quality.

For maximum strength in aerospace and high-load applications the 7xxx series applies, but the higher copper and zinc content demands attention to corrosion protection.

For brazed assemblies, silicon-bearing 4xxx filler and clad sheet are used rather than a structural alloy.

Confirm the temper as well as the grade, and ask for the mechanical property certificate against the delivery standard for the product form.

Frequently Asked Questions

Q: What does the first digit of an aluminium grade mean?
It identifies the alloy group. For example 1xxx is pure aluminium with at least 99.00% aluminium, 6xxx is alloyed with magnesium and silicon, and 7xxx is alloyed mainly with zinc.

Q: What is the difference between wrought and cast aluminium alloys?
Wrought alloys are shaped by rolling, extruding or forging and have good plasticity for pressure working. Cast alloys are poured into moulds and are grouped by their main addition, such as aluminium-silicon or aluminium-copper.

Q: What does the temper suffix mean?
It records the supplied condition. O means annealed, H means strain hardened, T means thermally treated and W means an unstable solution-treated state. The second digit gives the specific treatment level.

Q: Can the same grade have different properties?
Yes. Alloy chemistry is fixed for a grade, but temper changes strength, hardness and ductility substantially, so grade and temper must always be specified together.

Q: What are the old L, LF, LY, LC and LD designations?
They are legacy Chinese codes for industrial pure aluminium and for wrought alloy families: L for pure metal, LF for rust-proof, LY for hard, LC for super-hard and LD for forged grades. They remain on older drawings.

Q: Which aluminium series is most common for extrusion?
The 6xxx series, particularly 6060, 6063, 6061 and 6082. It extrudes cleanly, accepts anodising well and offers medium strength with good corrosion resistance.

Q: Which series has the highest strength?
The 7xxx series, led by 7075 and 7050. These alloys are used where load is critical, such as aircraft structures, and need protective treatment against corrosion.