Mar 07, 2024 Leave a message

Smelting Of 6063 Aluminum Alloy

Aluminum alloy smelting is one of the most important processes for producing high-quality cast rods. If the process is not properly controlled, various casting defects such as slag inclusions, pores, coarse grains, and feather crystals will occur in the cast rods. Therefore, it must be strictly controlled.

The melting temperature of 6063 aluminum alloy is preferably controlled between 750-760°C. If it is too low, it will increase the generation of slag inclusions, and if it is too high, it will increase hydrogen absorption, oxidation, and nitridation burning losses. Research shows that the solubility of hydrogen in molten aluminum rises sharply above 760°C. There are many ways to reduce hydrogen absorption when heat is used, such as drying the smelting furnace and smelting tools, and preventing the flux from being dampened and deteriorating. However, melting temperature is one of the more sensitive factors. Excessive melting temperature not only wastes energy and increases costs, but is also the direct cause of defects such as pores, coarse grains, and feather crystals.

Smelting of 6063 aluminum alloy

2. Select excellent flux and appropriate refining process

Flux is an important auxiliary material used in aluminum alloy smelting. The main components of the flux currently sold on the market are chloride and fluoride. Among them, chloride has strong water absorption and is easily affected by moisture. Therefore, the raw materials used must be dried in the production of flux. Completely remove moisture, seal the packaging, prevent damage during transportation and storage, and pay attention to the production date. If the storage date is too long, moisture absorption will also occur. In the smelting of 6063 aluminum alloy, the slag remover used, If refining agents, covering agents and other fluxes absorb moisture, the aluminum liquid will absorb hydrogen to varying degrees.

It is also very important to choose a good refining agent and a suitable refining process. At present, most of the refining of 6063 aluminum alloy adopts powder spraying refining. This refining method can make the refining agent fully contact with the aluminum liquid, so that the refining agent can perform better. Great efficiency. Although this feature is obvious, the refining process must also be paid attention to, otherwise the desired effect will not be achieved. The nitrogen pressure used in powder refining should be small, and it is better to be able to blow out the powder. If the nitrogen used in refining is not high-purity Chlorine (99.99% N2), the more nitrogen gas is blown into the aluminum liquid, the more moisture in the fluorine gas will cause the aluminum liquid to oxidize and absorb more hydrogen. In addition, the fluorine gas pressure is high and the rolling waves generated by the aluminum liquid are large, increasing the possibility of oxidized slag inclusions. If high-purity nitrogen is used in refining, the refining pressure will be high, resulting in large bubbles. The large bubbles will have great buoyancy in the aluminum liquid, and the bubbles will float quickly. The residence time in the aluminum liquid will be short, and the hydrogen removal effect will not be good, which is wasteful. Nitrogen, adds cost. Therefore, nitrogen should be used less and refining agents should be used more. Using more refining agents only has advantages and no disadvantages. The key points of the powder spray refining process are to use as little gas as possible and spray as much refining agent into the molten aluminum as possible.

Smelting of 6063 aluminum alloy

3. Grain refinement

Grain refinement is one of the most important processes in aluminum alloy casting, and it is also one of the more effective measures to solve casting defects such as pores, coarse grains, bright crystals, feather crystals, and cracks. In alloy casting, it is non-equilibrium crystallization. Most of all impurity elements (including alloy elements) are concentrated in the grain boundaries. The smaller the grains, the larger the grain boundary area. The concentration of impurity elements (or alloy elements) The higher the uniformity. For impurity elements, high uniformity can reduce their harmful effects, and even turn the harmful effects of a small amount of impurity elements into beneficial effects; for alloy elements, high uniformity can exert greater alloying capabilities of the alloy elements. To achieve the purpose of making full use of resources.

The effects of refining grains, increasing grain boundary area, and increasing element uniformity can be explained by the following calculations.

Assume that metal blocks 1 and 2 have the same volume V and are both composed of cubic grains. The side length of the grains of metal block 1 is 2a and the side length of 2 is a. Then the grain boundary area of metal block 1 is: Metal block 2 The grain boundary area of is: The grain boundary area of metal block 2 is twice that of metal block 1. It can be seen that if the alloy grain diameter is doubled, the grain boundary area will be doubled, and the impurity elements per unit area of the grain boundary will be doubled.